The wood samples were placed in the NaClO2 solution and kept boiling state for 2 h until the EW became white. Afterwards, the delignified wood samples were rinsed with DI water for three times and kept in ethanol. Subsequently, the as-prepared epoxy resin was used for thorough infiltrating into the delignified wood scaffold. Fabricated the…